Magnetic separation example of - 5mm granular ore entering PTMS magnetic separator
water cooling electromagnetic separator for Feldspar
When the concentrate grade reached about 53%, mineral recovery of 23.26% and yield of 13.09% when -1mm, recovery of 35.63% and yield of 18.94% when -5mm, the best choice of PTMS magnetic separator.
PTMS magnetic separator
It indicates that the separation effect of -5mm ore directly into PTMS magnetic separator after crushing is better than that of -1mm ore directly into PTMS magnetic separator after grinding. The main reason is that -5mm ore is not grinded, no mud, and high recovery rate. The production process is simple and the grinding cost is saved.
what is magnetic separation method for concentration of ore?
After a red ore concentrator adopts broken - 5 mm grade ore into PTMS magnetic separator magnetic separation, namely before grinding, sorting out the qualified concentrate conform to the principle of "to take early take" dressing, decrease the subsequent grinding, improve the processing capacity of the ball after grinding mill, effectively reduce the production cost, and prevent the useful mineral grinding so as to improve the recovery.
Contact: DELLA
Mob: +86-13929907491
sales@powtechina.com