The performance of high-gradient PTMS Magnetic Separator is better than others by improving whiteness
magnetic separation diagram
The dyeing impurities in kaolin (such as hematite, etc.) are weakly Magnetic, so it can be removed by using high-gradient PTMS Magnetic Separator, which can reduce the Fe2O3 in kaolin raw ore from 0.9% to 0.6% and Ti2O3 from 1.8% to 2.0% to 0.8%. This kind of high gradient magnetic separation with stainless steel wool as the medium, the field strength is 1.5 ~ 2.0T, needs 270 ~ 500kw power.
PTMS magnetic separator
PTMS has been tested by wet method, and good results have been obtained, especially for the removal of Fe Ti from kaolin by high gradient magnetic separation with vibration. Compared with the general Magnetic Separator, the performance of high gradient PTMS Magnetic Separator is better than others in terms of reducing the content of iron and titanium impurities and improving whiteness.
what is magnetic separation method for concentration of ore?
Because some iron impurities in kaolin ore exist in the form of silicate, the Magnetic is very weak, and titanium exists in the form of rutile, a single PTMS Magnetic Separator method is difficult to work, so the process is usually matched with flotation, selective flocculation and other operations to improve the quality of products.
Contact: DELLA