The process of calcination decarburization and whitening PTMS magnetic separator is used to solve the quality requirements of coated kaolin
feldspar mineral processing
According to the diagenetic characteristics of coal measure kaolinite, that is, it contains part of organic matter, and the raw ore whiteness is only 6% and 40%, which is far from meeting the quality requirements of paper industry for coated kaolinite. Therefore, the process of calcining, decarbonizing and brightening PTMS magnetic separator must be adopted. In the process of kaolin production, in order to avoid the formation of harmful mineral crystals (mullite and cristobalite), the calcination temperature is generally controlled below 1000℃.
PTMS magnetic separator
According to the different quality requirements of kaolin, PTMS magnetic separator treatment can be divided into two products: medium temperature calcined kaolin and high temperature calcined kaolin. The present calcining process can be divided into two kinds: molding calcining and powder calcining, each has its own characteristics.
how to separate two magnets?
There are many factors affecting the production process of coal measure kaolin PTMS magnetic separator, such as raw material quality, raw material particle size, calcination temperature, heating rate and constant temperature time, selection of additives and control of calcination atmosphere, etc. According to the characteristics of coal measure kaolin, according to the purpose of calcination, Appropriate calcination process parameters, processing equipment and technology should be selected.
Contact: DELLA
Mob: +86-13929907491
sales@powtechina.com