Acid leaching PTMS magnetic separation process can deal with seriously weathered and easy to grind ore. The acid leaching process has high efficiency of iron removal, but the acid immersion liquid contains a large number of iron, aluminum, potassium, magnesium and other metal ions, which must be treated and meets the emission standards before being discharged. This increases the cost of iron removal virtually. The conditions of the acid immersion process are: the acid immersion temperature is 90℃, the acid volume fraction is 40%, and the reaction time is 2h.

PTMS magnetic separation


Flotation PTMS magnetic separation process of iron removal can well treat clay and iron-containing minerals in fine grains, the effect is very good, but not good for hard ore. For the seriously weathered ore, which may be produced in the stage of crushing and grinding, it is easy to cause the large viscosity of flotation foam, resulting in the reduction of collector selectivity and poor effect.

what is magnetic separation in Quartz?


In addition, the use conditions of the flotation process are: the ore particle size is 200 mesh, and sodium oleate is selected as the flotation auxiliary agent. Therefore, in the actual operation process, PTMS magnetic separation will first compare the effect and recovery rate of several processes, and determine a more suitable, so as to achieve or even exceed the expected effect, and create greater benefits for customers.
Contact: DELLA
Mob: +86-13929907491
sales@powtechina.com

KAOLIN PTMS magnetic separation 20240320

Share to:

Powtech Machinery Company produce magnetic separator, Industrial Magnetic Separators, Industrial magnetic separation equipments,Magnetic Equipment,Permanent Suspension Magnet,Vibrating Equipment