How to separate iron impurities from kaolin by the PTMS Electromagnetic Separator chemical leaching method
published date: 2025/3/23
dry type magnetic separator
Chemical leaching method is to selectively dissolve certain impurities in kaolin by acid agents (such as sulfuric acid, hydrochloric acid, nitric acid) to achieve the purpose of removing impurities. PTMS Electromagnetic Separator The principle of chemical leaching is like dissolving unnecessary things with a "magic potion". Chemical bleaching is to oxidize impurities in kaolin into soluble substances by bleaching, and then removed by washing.
PTMS magnetic separation
PTMS Electromagnetic Separator In the process of chemical leaching method, different acidic agents have different dissolution capacity for different impurities. Oxic acid is a commonly used acidic agent that solves the iron ions on the mineral surface without affecting the lattice structure and physicochemical properties of kaolin. This is because oxalic acid has a special chemical structure, which can react with iron ions to form a soluble complex.
what is magnetic separation method for concentration of ore?
In practical application, when kaolin is mixed with oxalic acid solution and reacted under certain temperature and time conditions, the iron ions will be gradually dissolved in the solution, and then the solution is separated from kaolin by PTMS Electromagnetic Separator chemical leaching method, so as to remove iron impurities.