Feldspar Iron Removal: Laboratory Test at 60 Mesh, Before and After Fe₂O₃

Case study by FOSHAN POWTECH / PTMS · Published

Overview

This case presents laboratory test results for a feldspar sample at 60 mesh, submitted by FOSHAN POWTECH / PTMS. Sample A is the feed before iron removal, and Sample B is the material after iron removal. The analyses were carried out by an independent third-party laboratory, and the laboratory test was reported in 2025.

The original report does not specify the equipment or process conditions.

Test results

The table below lists the full chemical analysis for both samples, exactly as reported.

ItemSample A (before iron removal, 60 mesh)Sample B (after iron removal, 60 mesh)
Loss on ignition (IL)0.37%0.16%
Al₂O₃16.85%17.06%
SiO₂71.35%71.81%
Fe₂O₃0.37%0.03%
CaO0.67%0.66%
MgO0.35%0.04%
K₂O0.07%0.04%
Na₂O9.22%9.59%
TiO₂0.46%0.31%

Notes on the results

The original laboratory report states a particle size of 60 mesh, but does not specify whether the test was dry or wet, or the magnetic-separation conditions. The results are for reference only and are subject to a laboratory test on the customer's own sample.

Laboratory test results are not a guarantee of industrial-plant performance. Customers are welcome to send 5–10 kg for a free laboratory test; a report is issued within 5 days of sample receipt.

Test your own feldspar

Every ore behaves differently. Send FOSHAN POWTECH / PTMS a 5–10 kg sample of your feldspar for a free laboratory test, and we will share the full before-and-after analysis with you.