Factory-direct magnetic separators · Foshan, China[email protected] · WhatsApp +86 139 2990 7491

Case study

Feldspar Iron Removal: Laboratory Test at 80 Mesh and 200 Mesh, Fired-Cake Whiteness

Case study by FOSHAN POWTECH / PTMS · Published

Overview

This case presents laboratory fired-cake records for two feldspar samples tested by FOSHAN POWTECH / PTMS: one at 80 mesh and one at 200 mesh. Each sample was recorded as received (raw), after a first pass through a magnet, and after a second pass. Dry whiteness, wet whiteness and shrinkage were measured on cakes fired at 1200°C. Values are shown exactly as recorded.

These are laboratory fired-cake records, not third-party chemical assays. Each sample's results should be read only against its own raw, first-pass and second-pass values. The original records do not specify the equipment or process conditions.

Test results

The tables below list dry whiteness, wet whiteness and shrinkage, exactly as recorded. Empty fields in the original records are omitted and have not been estimated.

Feldspar, 80 mesh

Laboratory record, 2026. Two passes. Fired cakes at 1200°C.

Feldspar, 80 mesh: raw sample, laboratory fired cake at 1200°CFeldspar, 80 mesh: after the first pass, laboratory fired cake at 1200°CFeldspar, 80 mesh: after the second pass, laboratory fired cake at 1200°C

Left to right: raw sample; after the first pass; after the second pass. Laboratory fired cakes at 1200°C.

ItemRaw sampleAfter first passAfter second pass
Dry whiteness115062
Wet whiteness104551
Shrinkage-11-11-11

Feldspar, 200 mesh

Laboratory record, 2026. Two passes. Fired cakes at 1200°C.

Feldspar, 200 mesh: raw sample, laboratory fired cake at 1200°CFeldspar, 200 mesh: after the first pass, laboratory fired cake at 1200°CFeldspar, 200 mesh: after the second pass, laboratory fired cake at 1200°C

Left to right: raw sample; after the first pass; after the second pass. Laboratory fired cakes at 1200°C.

ItemRaw sampleAfter first passAfter second pass
Dry whiteness246475
Wet whiteness125368
Shrinkage-9-10-10

Notes on the results

These figures are laboratory fired-cake records (1200°C), not third-party chemical assays. They are for reference only and are subject to a laboratory test on the customer's own sample.

Laboratory test results are not a guarantee of industrial-plant performance. Customers are welcome to send 5–10 kg for a free laboratory test; a report is issued within 5 days of sample receipt.

Test your own feldspar

Every ore behaves differently. Send FOSHAN POWTECH / PTMS a 5–10 kg sample of your feldspar for a free laboratory test, and we will share the before-and-after results with you.


FARRALI

Send us your material. We test it free.

Send us 5–10 kg of your sample for a free laboratory test; report within 5 days of sample receipt. After the report, a matched model and price within 24 hours.

Free sample test Send an inquiry WhatsApp +86 139 2990 7491